  1. Okay well, 1/2 a tank later, I figured most of it...

    Okay well, 1/2 a tank later, I figured most of it out.

    Gas flow too low - Was 7-8Lp boosted it to 12
    Freq was low - went from 100 to about 140
    Pulled the AC balance up a little - Was at 90% now...
  2. Aluminum Tig welding - 1st attempt w/ PowerPro 205

    Hi Folks! Been a while since I logged in here but, since I have no pride anymore, here the question:

    I have now done dozens of steel projects with my 205. I has paid for itself at least twice....
  3. Replies
    39
    Views
    14,957

    Hi Folks, The DREAM CART build is under way...

    Hi Folks,

    The DREAM CART build is under way again. I'll have new pictures of the cart progress in about a week.

    What have I been doing? Well, I put an engine in son's car, closed my office...
  4. Greetings Jim and Welcome!! I do a bunch of...

    Greetings Jim and Welcome!!

    I do a bunch of busines with the company that puts your town on the map!
    The company I work for does all of their business television. Actually, I put Andrew on the...
  5. Liked on facebook....:D

    Liked on facebook....:D
  6. Looks great! Just a question: Is that intake...

    Looks great!

    Just a question: Is that intake shielded or high enough to keep it from taking a big drink of water?
  7. Replies
    39
    Views
    14,957

    So, the whole house now is wandering through the...

    So, the whole house now is wandering through the garage, asking questions about the new cart. My 14-year-old daughter asks, "Dad, where's the green tank go?" I said, Well, I'm getting another, larger...
  8. Replies
    39
    Views
    14,957

    Well, I was born when my dad was 52. My dad was...

    Well, I was born when my dad was 52. My dad was born in 1908.
    Most of his service was in the South Pacific aboard a sub tender before I was born. http://www.navsource.org/archives/10/19/1941.htm
    I...
  9. Replies
    39
    Views
    14,957

    Not a windows fan either. However, my dad once...

    Not a windows fan either. However, my dad once told me, "Son, you do the very best you can with what you've got or, have been given..." I find this sage wisdom for all aspects of my life. The wife...
  10. Replies
    39
    Views
    14,957

    I have one much bigger than this at my office - I...

    I have one much bigger than this at my office - I still use it. When the EMP hits, the folks fluent in autocad will be out of luck!:D
  11. Replies
    39
    Views
    14,957

    The front frame will accomodate a 19" rack-mount...

    The front frame will accomodate a 19" rack-mount device or drawer. I may (from your comment) "inset" the rear wheels now to reduce this profile as it is only a tank deck.
    THANKS!
  12. Replies
    39
    Views
    14,957

    Good point! I will need to add a tube for filler...

    Good point! I will need to add a tube for filler rods! THANKS!:D
    This is actually a very nice cart!
  13. Replies
    39
    Views
    14,957

    I used Microsoft Visio to draw it. Been using it...

    I used Microsoft Visio to draw it. Been using it for about about 15 years - as long as it has been out and before it was bought by Microsoft.
    The I took a picture of my PowerPro 205 at the same...
  14. Replies
    39
    Views
    14,957

    I haven't welded anything in about 15 years. What...

    I haven't welded anything in about 15 years. What fun would it be to put together a cart from Harbor Freight? Like I said, I've got some spare time coming up this spring.

    After all, I'm a...
  15. Replies
    39
    Views
    14,957

    My son and I are both 6'5" tall.:P Anybody...

    My son and I are both 6'5" tall.:P

    Anybody know off-hand what the height and diameter of a 125CF? Diameter is the most important as I will need to adjust the rear foot and cage dimensions and also...
  16. Replies
    39
    Views
    14,957

    More details... As other folks are saying, I'm...

    More details...

    As other folks are saying, I'm probably going to get a larger tank at some point. I was trying to future-proof it as much as possible. The top shelf is 19" wide - same width as the...
  17. Replies
    39
    Views
    14,957

    Everlast "Dream Cart" - Under Contruction

    Well, I started welding this up today. I'll post pictures as it gets closer to being "real".

    Comments, questions and suggestions welcome...

    Finally!

    6353
  18. Replies
    23
    Views
    14,605

    You know, it would be really great if Everlast...

    You know, it would be really great if Everlast opened an EAST COAST repair facility. **hint-hint**

    Also, and, not that I encourage anyone to open and try diagnosing problems with their own...
  19. Replies
    20
    Views
    6,977

    Had the same condition on my PP205. I even asked...

    Had the same condition on my PP205. I even asked the salesman about it after it was delivered - thinking it had been tossed by one of the UPS trucks. It has worked just fine - no problems. Don't...
  20. Replies
    55
    Views
    20,764

    $139 on ebay ...

    $139 on ebay

    http://www.ebay.com/itm/DSA50SE-SK2-FULL-SET-INDUSTRIAL-GRADE-3L-3-17QT-250W-DIGITAL-ULTRASONIC-CLEANER-/290604862797?pt=LH_DefaultDomain_0&hash=item43a9664d4d

    not very big but...
  21. Many thanks! You know, there are probably a dozen...

    Many thanks! You know, there are probably a dozen possible combinations that will work.

    I wish I had taken a picture of the root pass. It was awesome! As I said, this was the 3rd weld on this...
  22. Replies
    7
    Views
    2,688

    I guess this would depend on how dusty the...

    I guess this would depend on how dusty the environment stays. Just be careful not to pull anything lose, and be VERY CAREFUL nothing is pinched between the case when it goes back together. A pinched...
  23. PowerPro 205 - first BIG welds - porosity issues resolved

    Well, the issues I had with Porosity are now gone. Seems like there were a host of little thing that were working against me. Any one of them could have caused the problem. Hoses, insificient...
  24. Replies
    13
    Views
    3,492

    Good review.

    Good review.
  25. Replies
    14
    Views
    3,747

    This is a GREAT tip! Never though of this but it...

    This is a GREAT tip! Never though of this but it makes complete sense. THANKS!
Results 1 to 25 of 63
Page 1 of 3 1 2 3