That was it! One of the connectors to the trigger inside the gun had slipped off. I love when a problem turns out to have a simple solution. Rarely the case for me...
And in answer to my own...
Type: Posts; User: mak
That was it! One of the connectors to the trigger inside the gun had slipped off. I love when a problem turns out to have a simple solution. Rarely the case for me...
And in answer to my own...
I was using the plasma cutter on my PP205 and it suddenly stopped working. I had made one cut about 10" long through thin sheet metal. Started another cut and it would shoot a single hole through...