Search:

Type: Posts; User: Andyco

Search: Search took 0.01 seconds.

  1. Replies
    3
    Views
    7,164

    It seems the problem with the display has fixed...

    It seems the problem with the display has fixed itself. Used welder to repair a broken truck frame. Display worked properly. Go figure!
  2. Replies
    3
    Views
    7,164

    I mig 200 display problems

    Got another problem guys: Been doing some build up on a suspension equalizer on one of my truck. Ran about six 3" long beads and around five 1" long beads using 15.5 volts and around 215 wire speed....
  3. Replies
    16
    Views
    17,492

    Got another problem guys: Been doing some build...

    Got another problem guys: Been doing some build up on a suspension equalizer on one of my truck. Ran about six 3" beads and around five 1" beads using 15.5 volts and around 215 wire speed. After the...
  4. Replies
    16
    Views
    17,492

    Now we're talking. Thanks Oleg et al.

    Now we're talking. Thanks Oleg et al.
  5. Replies
    16
    Views
    17,492

    Mark: Sent the welder in question by UPS to your...

    Mark: Sent the welder in question by UPS to your service center in Idaho on Nov 28 and was confirmed delivered on Dec 3 by tracking # 1Z7106AX0343495675.
    I called Ray in tech support on Jan 8 and...
  6. Replies
    16
    Views
    17,492

    Got my return # today. I'm not in the clear about...

    Got my return # today. I'm not in the clear about what to return. The main unit of course, but how about the mig and stick leads and the ground lead?? I will be removing the OSHA plug.
  7. Replies
    16
    Views
    17,492

    Mike R: Checked both terminals from the power...

    Mike R: Checked both terminals from the power out side of the on/off switch and had 115/120 on both. ..................Mr Murphy: Could only find one fuse and it was ok..Looks like tech support in...
  8. Replies
    16
    Views
    17,492

    Tried stick mode. Switched ground to neg. No...

    Tried stick mode. Switched ground to neg. No help..... And to answer Mark, the green "on" lit is on (the upper one). I'm out of idea's. Anybody????
  9. Replies
    16
    Views
    17,492

    Hey DaveO: Thanks for the welcome. Yes, positive...

    Hey DaveO: Thanks for the welcome. Yes, positive ground. Plugged in and turned the ground plug to the machine a couple of times to make sure was connected ok. Tried arcing to ground clamp and to the...
  10. Replies
    16
    Views
    17,492

    I mig 200 won't arc

    Sirs: Purchased an I mig 200 about 1 1/2 years ago and have been very pleased with performance until recently. I was stich welding some sheet metal with flux core (all my welding is outside and...
Results 1 to 10 of 10