Search:

Type: Posts; User: bigun12

Search: Search took 0.00 seconds.

  1. Replies
    5
    Views
    14,640

    Oh it is! And very much lighter then my other...

    Oh it is! And very much lighter then my other (Miller) machine. I have also noticed that I can produce very similar beads to the ones I make with the Miller machine at quite a bit lower amperage...
  2. Replies
    5
    Views
    14,640

    1351613517 As requested photos attached.

    1351613517

    As requested photos attached.
  3. Replies
    5
    Views
    14,640

    First review of new Power Ultra 206PI

    Had it a couple of weeks now and thus far have cut some 1/2" plate (like butter) and welded it together with some 1/8th" 6011 at about 110 amps and a few 7014s at about 100 amps!

    Beautiful! I...
  4. I recently bought a PowerUltra 206PI mainly for...

    I recently bought a PowerUltra 206PI mainly for the Plasma cutting ability but having the Tig and stick capabilities included is a REAL plus. I haven't had occasion to do much with mine yet other...
  5. Replies
    4
    Views
    4,179

    Yes! The manual says to open the machine up and...

    Yes! The manual says to open the machine up and blow it out with air periodically. Is that just a matter of taking out the four screws on the sid of the machine and lifting the cover off?
  6. Replies
    4
    Views
    4,179

    Thanks! Got it downloaded.

    Thanks! Got it downloaded.
  7. Replies
    4
    Views
    4,179

    Howdy from a new Everlast user in Texas.

    A BIG Texas HOWDY!!!

    September 30, 2016 I ordered a Everlast PowerUltra 205P from Sears Roebuck and Company. On October 9 2016 the package arrived intact via UPS. The package contained a brand...