Search:

Type: Posts; User: Longlasting

Search: Search took 0.00 seconds.

  1. Replies
    20
    Views
    11,045

    Pot schematic

    4019Here is a pot schematic and it is a 50 k pot to test with an ohm meter.If you want to go to a Miller style check out scc electronics, they have everlast pedals.
  2. Replies
    28
    Views
    13,172

    electrode size

    Got gas coming then....on metal approaching thickness at 1/8 to 1/4 you should be changing over already from Ceriated or 2%lan. to 1/8 electrode size, you have the collets you need with your kit and...
  3. I did one of my machines in the winter, but the...

    I did one of my machines in the winter, but the supplier of infineon mosfets expect you to buy a lot of 100 so I bought 2.Cost $10.00 cdn $25 for shipping and wire transfer.I love the fact that I...
  4. Replies
    4
    Views
    9,906

    Chinese copies

    I have all winter to fix the board or the welder, it is not the only unit I have and want to use it on a home built cnc plasma in the spring(24x48), I have all winter to do the boards for that too....
  5. Replies
    4
    Views
    9,906

    No, it is not, but I'll call you direct,...

    No, it is not, but I'll call you direct, appreciate any service help.I herniated three vertabrae in my back and cannot lift, so moving it is out of the question.Got a surgical consult setup.
    It is...
  6. Replies
    4
    Views
    9,906

    Service Manuals

    Does anyone know if their are any service manuals/schematics available for the 200amp multifunction welders, so that their is a way of testing the boards to self diagnose the problems.I used to...
  7. Replies
    9
    Views
    7,167

    Sharpening tungsten

    Get yourself a grinder and resurfacing wheel, doesn't have to be an expensive grinder but one with a light is good.Hold the tungsten between your finders to steady and with other hand turn the...
  8. Replies
    8
    Views
    5,533

    Welding Fitting

    Get rid of that 1/16 tungsten, be surprised if you are not melting it or burning it awaytrying to get the heat you need, try 3/32 ceriated.Absolutely forget pulsing for now I'd bet your heat is way...
  9. Replies
    13
    Views
    16,448

    Regulator failure

    Actually this is the first I have heard of regualtor failure from not bleeding off the regulator, when I was in trade school in the 80's I remember being taught to bleed off oxyacetylene lines as a...
  10. Replies
    9
    Views
    6,102

    Fixing rivets

    You can get a tool for tightening rivets at a mack of kenworth dealership, it is a dolly with a divet cut into it and an air chisel blade if I recall right.
  11. Replies
    13
    Views
    16,448

    Argon/Air Leaks Repaired

    No it is not bad right now in fact it is liveable, on my mig I shut down the gas and leave it I don't bleed the mixed gas, and you think this would be the same.One would think if I can get the T/A...
  12. Replies
    13
    Views
    16,448

    Argon Leaks

    Well what I did was remove the cover and take some soapy water and pressurized the line with air to 110psi, and I found a very large leak at the solenoid and a loose nut at the pressure gauge.So I...
  13. Replies
    13
    Views
    16,448

    Argon gauge questions/ball type flow meter

    I am using a quick connect to connect and disconnect the argon from the air line on my multi function machine and I am using the ball type flow gauge it came with; my mig has the twin head flow gauge...
  14. Replies
    13
    Views
    6,454

    Poof!!!

    No it is a new unit.Leave it at that. I am just quite upset at UPS because I have searches about these import machines, through alot of threads and the biggest failure rate of these units seems to be...
  15. Replies
    13
    Views
    6,454

    Overheat lamp and strange sound?

    Hi I have had an overheat light on my machine a 200 amp import, ups dropped the package in delivery(idiots) and dented the back panel, but it was all intact inside, tried it out, everything worked ok...
Results 1 to 15 of 15