    Miller XMODE

    I have the digital elite.
    Powertig 250ex.
    Down to 5 amps works perfect but.
    I only use x mode it triggers from the high freq.
    So it seems the Elite does not care if there are any amps at all it...
  2. Replies
    1
    Views
    3,055

    Thanks for the tip

    Thank you for the heads up. I had hooked mine up as the book showed.
    With the Nova torch you are 100% correct and when I read your post that got me checking.
    Thanks to you my torch is now hooked up...