  1. 5 month old PowerTig 250EX and heres what I think

    Hello all,

    As the title says I have owned my PowerTig 250EX for roughly 5 months now and I have to say that this unit is awesome! I weld a variety of materials, mostly stainless, and this machine...
  2. Thread: New 250EX

    by Gustaf
    Replies
    7
    Views
    4,319

    Sorry to say the A/C buzz never goes away. You...

    Sorry to say the A/C buzz never goes away. You want it to sound like an angry bee. I wear earplugs and it helps a little on the noise. Steel is definitely more forgiving than aluminum. I enjoy the...
  3. Thread: New 250EX

    by Gustaf
    Replies
    7
    Views
    4,319

    This could be unrelated but might also be...

    This could be unrelated but might also be helpful.

    Are you using the provided foot pedal? Have you tried using your torch trigger switch instead of your foot pedal? I ask because I purchased a...