    11,643

    Well, I think getting curly turns is common thing...

    Well, I think getting curly turns is common thing while drilling in steel. I also experience this thing already and its nothing to done with efficient work. You can do it with your expertise only.
  2. Replies
    13
    Views
    12,834

    If a defective welds discovered after a structure...

    If a defective welds discovered after a structure is complete, the weld must be removed and the entire welding work to be redone, so eat your profits and valuable time. This is little bit important...
  3. Thread: My Welds

    by martinnman
    Replies
    35
    Views
    19,902

    You'll probably need to change the temperature...

    You'll probably need to change the temperature and rate of thickness change, the more you have to be a lot of grinding to do.
  4. Replies
    14
    Views
    7,617

    Check your freon levels if your cooler is not...

    Check your freon levels if your cooler is not providing you with cold water any longer. If it appears that there is a problem with Freon, you need a professional to fill the freon. Only those with...