Thanks guys! I think the progress with steel is good but with aluminum (AC) still bad. The arc is inestable all the time and the rod jump all the time when i want the fusion. I swapped again with DC...
Type: Posts; User: alfweld
Thanks guys! I think the progress with steel is good but with aluminum (AC) still bad. The arc is inestable all the time and the rod jump all the time when i want the fusion. I swapped again with DC...
My progress with steel
Before:
http://i283.photobucket.com/albums/kk303/alfsentra/20140706_174915.jpg
After:
http://i283.photobucket.com/albums/kk303/alfsentra/20140704_184213.jpg
...
I'm back and here is my first steel practice:
http://i283.photobucket.com/albums/kk303/alfsentra/steelpractice.jpg
Here is my argon tank:
http://i283.photobucket.com/albums/kk303/alfsentra/20140605_183559.jpg
Trying! Looks HORRIBLE :D I dont know why!...
Sorry! Yes, is "melt". I have a 6 cup in my torch. Maybe i have too much gas flow (18 LPM) for this cup? I have 1/8" rods and for clean the aluminum i use a steel brush and acetone. Any other...
I have a question all time in my head... Why i can't have a good arc? I cleaned and used the red (recommended) electrode but with the same bad results. Other is why when i want add the rod to the...
I have familiarisation with... Hehehehe!!!
I need practice and practice and practice ;-)! I'm searching a local school to take class.
I'm done. I practiced with steel and looks "little decent" but in AC with aluminum is horrible. I damage again the tip of the electrode and the arc is horrible, never stabilized. I saw videos, read...
Good news! I changed the terminals and now are correct. I'm practice with steel and looks good. More posts and questions soon! Thanks guys!
My bad.... Sorry guys! I check again this night!
Thanks!
I'm using brand new 100% argon gas tank.
Here is the other parts:
http://i283.photobucket.com/albums/kk303/alfsentra/20140605_183615.jpg
...
Again here with bads results. I bought a red electrodes (3/32" x 7") and i fried 4 inches! I have a ball in the tip and i dont know what happened. I think is a 90% my fault but im feel frustrated. I...
Thanks guys! I check the blue electrodes today in the local shop and more practice in the afternoon. More posts soon!
Thanks!
I'm back guys but a little frustrated! I have green electrodes 3/32x7 and i fried 2 and i dont know why. I don't have a stabilized arc, i damage a #6 ceramic cup, i tried differents settings, set to...
Electrodes ordered! I'm reading about and waiting for the electrodes for practice. More posts soon! :-)
Thanks!
Hi guys!
I bought a Everlast 185 AC/DC tig welder few days ago. I never welded with tig, i only have a little idea. I read and saw videos about tig welding and differences of adjust in the...