Will Everlast ever design a full all in one machine with 120/240 TIG (AC/DC), MIG, STICK, and PLASMA? I really like features of the POWERMTS models but cannot find myself purchasing one because it...
Type: Posts; User: scootarida1
Will Everlast ever design a full all in one machine with 120/240 TIG (AC/DC), MIG, STICK, and PLASMA? I really like features of the POWERMTS models but cannot find myself purchasing one because it...
Torch is the S45
Yeah I was glad to.
FWIW if you go into the wood section with the select wooden boards, there are some smaller 3/8" thick boards I found and used my miter saw to cut some 45* into them and then...
Well I thought I'd post up on my results.
Turned all of the knobs to 0 except the amperage setting I wanted to run. I was able to run the machine perfectly. Cut up a bunch of 1/8" angle to make...
CK 130 superflex ftw!
Post some pictures up of what they look like when your done.
Yep switch to AC for aluminum and make sure your balance is around 20-30 if the material is clean. To much balance will destroy electrodes quickly. Depending on what weld joint, adjust the AC...
Good to know, I will deffinately post back on here when I get a chance to try the knob trick. If it does turn out to be the fix, it is probably something worth mentioning in the instruction manual.
Alright let me know how it works
It does stay active in pulse on my machine.
I was playing around with my PP205 doing some stick and realized I had left the pulse feature on from TIG. When doing stick it still was pulsing and just wondering if there is any advantage of...
Nice buy, I actually was going to purchase one of these 185s but ended up getting the PP205. Most of the time I don't even use the pulse features, just the basic controls.
Unfortunately I have not had time to test as Im back to college. I was just home for a break to make something. I will try it sometime in December and get back to you. I am going to try the knob...
No I did not change any of the other knobs. I can give that a try and see what happens.
I found myself running into a problem and maybe someone can help me out.
When I try plasma cutting, sometimes it will cut fine and sometimes it will pilot arc and then goes out and sets off the...
He just wondering a little about this setup. Are the fittings 1/4 npt or 1/8 npt. Also did you buy a tee for high pressure rating or is that not needed?
I made pig tails for my I-Mig 200 which is dual voltage. Used the L6-30 twist lock style. I used a male end off of the machine and then used female ends for the 120 and 220 pigtails. Just make...
Sorry to thread jack but do these fit on the Power Pro 205 Plasma torch.
Thanks for posting this. I just ordered one of these. It was a little bit more than yours maybe $5-10 but still will be much better than my wp-9/17 harbor frieght tig torch I am using. I rarely...
I used the powerpro 205 tig for the catch can project. Also for that material I used a foot shear to cut the metal. It cuts nice and straight. However can you use ur bandsaw in the vertical...
I recently purchased a I-Mig 200 and I was surprised how smoothly it welded. Even if the settings weren't perfect, it welded nicely.
For the 1" to 1/8" you will want to preheat the 1" or else...
On your inside corner joints for Aluminum, your going to want to make sure the tungsten is closer to the joint and you increase your AC frequency to help focus the arc down into the corner. I've had...
Yup that what I was wondering. I might have to go pick one of those up
what department did you purchase that from?
I'm in at 125 posts. I should have some good stuff coming up. Should have a welding cart for my PowerPro 205, a nice welding table, and a cart for a miller 211 that I am purchasing this week. stay...