  2. I"m not sure, but here in the US, the ipt60...

    I"m not sure, but here in the US, the ipt60 torches are more widely available. Everyone seems to be using that torch outside of the Miller/Hypertherm/Victor names in one form of the other.
  3. Replies
    12
    Views
    394

    And now we've refined the hood itself.

    And now we've refined the hood itself.
  4. Replies
    8
    Views
    186

    A lot of people "ignore" the inductance/arc force...

    A lot of people "ignore" the inductance/arc force control and set it to 0. That is a huge mistake. Set it for about 65 to 75% and you'll do a lot better and settings will perform better.
  5. Replies
    8
    Views
    186

    The unit is especially difficult to set for...

    The unit is especially difficult to set for Aluminum. There is no hot start for the unit. It is best used for steel and stainless applications in Pulse.Again, the Power i-MIG 253 is designed for...
  6. Replies
    8
    Views
    186

    The 275P is designed for highly experienced...

    The 275P is designed for highly experienced welders. Pulse is really set along a complex logarithmic line of multiple variables. It can be set manually, if a person is experienced, but a chart is...
  7. Replies
    5
    Views
    137

    Which business hours? Tech support works East...

    Which business hours? Tech support works East Coast hours. Call me today. If you leave a message (providing you can't get me) I'll call you back, even after hours.
  8. Replies
    8
    Views
    208

    Arc wandering is the arc looking for a circuit...

    Arc wandering is the arc looking for a circuit path. May be due to a bad work clamp, or an improper clamp location or other operator/environmental issue. If the arc is on, it shouldn't be a welder...
  9. Replies
    8
    Views
    208

    AC has never been an issue with an inverter as...

    AC has never been an issue with an inverter as far as I know. NOt in modern times, (last 20 years). But arc starts usually have to do with work clamp location/condition and other settings...not the...
  10. Replies
    8
    Views
    208

    How old is it?

    How old is it?
  11. Replies
    8
    Views
    544

    Sounds like junk to me.

    Sounds like junk to me.
  12. 14 to 104 F operation. Storage at 40 below is...

    14 to 104 F operation. Storage at 40 below is not recommended.
  13. ESAB atom arc is one that comes highly...

    ESAB atom arc is one that comes highly recommended by several that have tried it.
  14. Replies
    5
    Views
    216

    It's fine, it'll be sort of a soft arc.

    It's fine, it'll be sort of a soft arc.
  15. Replies
    5
    Views
    216

    Usually wrought iron does present issues with...

    Usually wrought iron does present issues with welding. It is super high in carbon and having welded it myself, you need to turn up the heat, and focus the heat on the wrought iron (many times it is...
  16. Apologies. A couple of things you should...

    Apologies.

    A couple of things you should keep in mind. Keep the rod buried. Don't take it out of the puddle. Make sure you have the work clamp directly connected to the part being welded.
    ...
  17. Replies
    1
    Views
    170

    If you use the unit like it is designed to be...

    If you use the unit like it is designed to be used (stacked under the 275, directly to it) then nothing will get caught on the cooler fill neck because your work and torch leads stick out further. ...
  18. Replies
    8
    Views
    544

    I don't see why not.

    I don't see why not.
  19. Just one post is sufficient. See my reply to the...

    Just one post is sufficient. See my reply to the other post you made. My thoughts are along trying a different/better brand.
  20. Replies
    5
    Views
    216

    Turn on 6010. But your amps are a bit low. Try...

    Turn on 6010. But your amps are a bit low. Try 80A. What brand rod? Hobart?
  21. Replies
    8
    Views
    544

    Call the manufacturer. Don't rely on "others" to...

    Call the manufacturer. Don't rely on "others" to inform you. We've seen misinformation before on this stuff.
  22. Replies
    8
    Views
    544

    Northern Tool powerhorse line. They have a...

    Northern Tool powerhorse line. They have a 13000w one about that price. Meets the requirements. A lot of the cheaper products say they are but aren't. If it's duromax or champion, be very careful...
  23. Replies
    12
    Views
    3,212

    Call 877 755 9353 ext 207 tomorrow 9 to 5...

    Call 877 755 9353 ext 207 tomorrow 9 to 5 eastern. Don't delay. If it hasn't been 5 years it should be under warranty. If it has it can be fixed for a reasonable price in comparison to purchasing...
  24. Replies
    12
    Views
    3,212

    Make sure you didn't drop your swirl ring out.

    Make sure you didn't drop your swirl ring out.
  25. Replies
    12
    Views
    3,212

    If it has HF start, then you may have a Plasma...

    If it has HF start, then you may have a Plasma inverter problem. Make sure you have the torch on the negative when you cut. Select 2T.
Results 1 to 25 of 500
Page 1 of 20 1 2 3 4