Just giving my experience with this thing.
Type: Posts; User: dgrue
Just giving my experience with this thing.
I shouldn't have said arc starts. Arc wandering was more the issue: same torch, different welder = more stability. Which in some sense is no longer any issue: no arc = no wandering! I cover up my...
Purchased in 2013.
Yeah, people like you and me pay them by buying their equipment! I'm trying to minimize that by accessing the collective wisdom here.
Bought new. Worked okay. Never great at starts. Arc would take...
Technically it's not 'dead'--the machine turns on. But effectively it is: no arc.
HF works, but the arc won't fire. Same with lift/scratch: no arc. It doesn't seem to be a cable or control issue:...