Search:

Type: Posts; User: johnson697

Page 1 of 9 1 2 3 4

Search: Search took 0.01 seconds.

  1. Replies
    5
    Views
    8,295

    was thinking on getting this machine...was mostly...

    was thinking on getting this machine...was mostly gonna be cutting 1/8 5052 aluminum ...some are gonna be long cuts but must of them will be 6 to 8" holes...i know aluminum is a little harder to cut...
  2. Thread: imig205

    by johnson697
    Replies
    5
    Views
    6,315

    glad to hear that ive had my machine 5 yrs now so...

    glad to hear that ive had my machine 5 yrs now so no warranty and i love the machine...its done all ive ever asked of it...hope this is all it is.
  3. Thread: imig205

    by johnson697
    Replies
    5
    Views
    6,315

    i had talked to mark also and he thought the same...

    i had talked to mark also and he thought the same as you stated but wasnt sure ...will wait for response back from techs to see if it is the same...did you get schematics on where to place the...
  4. Thread: imig205

    by johnson697
    Replies
    5
    Views
    6,315

    imig205

    having a problem with tack welding...i tack about 4 or 5 times and over current light comes on and wont weld but still feeds wire,so i turn machine off and start to weld and no problems but when i go...
  5. Thread: 315 lx

    by johnson697
    Replies
    10
    Views
    15,451

    bought this machine last week and it is on back...

    bought this machine last week and it is on back order...replacing my 250 ex...the 250 was a great machine but ran into a few times needing the extra amperage .cant wait.
  6. Replies
    25
    Views
    12,159

    used a 375 aspect this winter at a trade...

    used a 375 aspect this winter at a trade show....liked it alot ..could have bought it for 5600.00......friend of mine made the fuel cell for a gt-40 was really sharp....i make reservoir tanks for...
  7. Replies
    13
    Views
    12,874

    did i read that right for types of wire?5356 and...

    did i read that right for types of wire?5356 and 4053 for aluminum on the front of panel?
  8. Replies
    6
    Views
    4,561

    Watching a few videos on the 255 and although i...

    Watching a few videos on the 255 and although i dont NEED to have a 255.Doing different jobs at home i could see where having a machine like this would be beneficial in making a job a little easier...
  9. Replies
    6
    Views
    4,561

    what kind of work do you do with it?how thick of...

    what kind of work do you do with it?how thick of material?
  10. Replies
    6
    Views
    4,561

    255 tig question?

    i was considering buying the 255 and wanted to know the capabilities of the 255 over the 250...will be welding mostly aluminum.125 to .250 5052.?i own the 250 and am very happy with it but was very...
  11. Replies
    4
    Views
    8,147

    what foot pedal does the 160sth use...i have a...

    what foot pedal does the 160sth use...i have a 250ex...will the foot pedal work on the 160sth?
  12. for home use the 140e is a great little 110...

    for home use the 140e is a great little 110 unit....you would be surprisewd what this little machine can do....and if you want to get into aluminum tig the 250 ex is a very nice machine have had 1...
  13. Replies
    3
    Views
    3,971

    yes homemade grill...made 2 of them now.

    yes homemade grill...made 2 of them now.
  14. Replies
    3
    Views
    3,971

    140e awesome little welder

    everytime i use this little welder it impresses me everytime...did this today with the 140.13081
  15. wanna trade?

    wanna trade?
  16. ive also had bad argon tanks to...happens when...

    ive also had bad argon tanks to...happens when people empty the tank all the way...should never do that and also people leave the valve open on the tank when they return it...that will contaminate...
  17. 13077welded this with my 250 ex...would love to...

    13077welded this with my 250 ex...would love to try 1 of the 255 tig welders..
  18. Replies
    5
    Views
    4,736

    a baseball bat ....yep thats what i would do to...

    a baseball bat ....yep thats what i would do to ...both knee caps...ive had stuff stolen from garage too....glad i didnt have a gun and caught them red handed ...id be in prison for sure.
  19. Replies
    4
    Views
    8,147

    wanting to buy stick welder

    looking to buy a stick welder and wanted to know what size genarator i might need for either the 160sth or 200?never done any stick welding but i live in farm country and want to do repairs for...
  20. Replies
    24
    Views
    11,857

    so what was wrong with the unit?

    so what was wrong with the unit?
  21. Replies
    16
    Views
    6,949

    did you dip your tungsten...your welds look a...

    did you dip your tungsten...your welds look a little contaimanatiated...what size and type of tungsten are you using ?are you sharpening your tungsten properly?
  22. Replies
    12
    Views
    14,262

    a little high on price as i can get a new 1 for...

    a little high on price as i can get a new 1 for 2200.00.what is reasonable?
  23. Replies
    3
    Views
    3,725

    its the plan jane version ...no pulse or anything...

    its the plan jane version ...no pulse or anything else....i have used 1 for the past 16 yrs . and it has all the bells and whistles...but i see your point on this and have decided not to get it...but...
  24. Replies
    3
    Views
    3,725

    miller aerowave vs. 250 ex

    I have a chance to buy a miller aerowave for 1750.00 with torch ,foot pedal and water cooler....but if i buy this i have to sell my 250 ex ...love my 250 but the aerowave is a badass machine...whats...
  25. Replies
    12
    Views
    14,262

    what all comes with it ?is this your bottom...

    what all comes with it ?is this your bottom dollar?
Results 1 to 25 of 215