11 Attachment(s)
Same thing, different day
Yet another Kubotoa RTV conversion. This one is a little different. Larger tank than last time and everything mounted up higher for more destructive areas. Found some real aggressive tires to give it some more bite, too.
The original plan...
Attachment 13384 Attachment 13383 Attachment 13382
Here is the basic framing. You can see I had to do a little heat straightening on a few pieces after the welding. Next time I need to plan out the order of welding a little better.
Attachment 13388 Attachment 13387 Attachment 13386 Attachment 13385
And the finished product. Stayed pretty close to the plan. This time I added a hydraulic lift to make service a lot easier.
Attachment 13392 Attachment 13391 Attachment 13390 Attachment 13389
Pretty much all the welding was done with my little PA140 in TIG mode.