PowerTig 255EXT welding power problem
I was welding a part and put it on the work bench to finish welding it and the welder stop working made a sound like it was going to work but didn’t. Moved it off the bench to see what happen to the welder holding the part in my hand with the ground clamp still on it and it started working again so I put it back on the bench to finish welding it and it stopped again. Moved it off the bench again and it welds OK.
So on the work bench it will not weld still with the ground camp on the work piece I was welding. Take it off the bench it works on the bench it will not work weld and the ground clamp is always on the piece I am welding, I never take off the part.
So out comes PowerTig 250EX to see if it will work and it dose on or off the bench using the same settings same piece same gun and ground clamp.
The MTS 250S works on or off the bench.
The PowerMig 250 works on or off the bench.
The PowerTig 255EXT will not weld on the work bench.
Tomorrow it will try again.