Yes, that's a little strange. I don't know if this helps, but on my 255 I also had arc fluttering on low amps. I found out if the tungsten is too big and if the amps are set too high it will cause this. For instance if the machine is set at 200 amps and the pedal is pressed 1/4 of the way down you would have about 50 amps, if it was set at 50 amps, 1/4 would be about 12 amps. This has a big affect on small movements. It's better to set around 25amps then floor the pedal and then back off when the arc is established. I am able to weld on the bottom of soda cans, but cannot even begin to weld two together. As you said, the arc jumps from side to side then it just blows a hugh hole in the can. I figured it's just my lack of experience, maybe some day. The machines are really really good, just not great. I hope you get your issues resolved.