Originally Posted by
JimMinKent
Oh boy, you just got me thinking...
With all the timers on board the EXT, a guy should be able to spot weld, And We Can!
For a say, 60 amp 2 second spot weld do this:
2T mode
AC or DC your choice,
Pre-flow = 0.5 (my standard setting)
Start amps = 60
Upslope = 0
Welding amps = 60
Downslope = 2.0 sec
End amps = 60
Bingo, just let off the switch as soon as she lights off, and you've got a burn time the duration of your Downslope setting.
These machines are SOOOO cool :D
I had never known of that trick on the Syncrowave crater fill/HF operation, nice little trick. Now had you been able to set the target ending amperage with the crater fill, you'd have had spot welding there, too. That option is not installed on my SW, and always made me want to get it just so the panel had all the knobs! But not so much any more. :cool:
Here she is on display in my shop, hasn't had any use since my Legacy EXT showed up.