clamp in (work) - pulse seems to help on flat surfaces but no not using it now trying to get it to weld proper without first. tried
Steel %75ar-%25co2 .035 1/8-1/2 in thickness all kinds of combinations of V and amperage always starting with the recommended settings and slowly moved around from there.
Aluminum %100 ar spoolgun .8mm wire .090-1/4 in thickness all kinds of settings and thicknesses always starting with recommended, same result piles up on the surface or jumps to spray arc and melts to a ball 1/4 away from work and flows with gravity from there only looks good on flat steel cant really put it where you want it
I have worked as a mig welder in the past so I have experience adjusting mig machines, also used to build aluminum awnings for another company using a spool gun everyday
I still have to put the tie bar in for the awning caves I really dont want to have to tig weld the 125ft of 3/4 by .090 aluminum square tubing thats what I bought the mig for
is there any way to adjust the wire speed without messing with the amps?