Are the pieces of clear reinforced hoses included with the unit(s) suitable for argon and/or compressed air?
What is the pressure rating?
Thanks!
Printable View
Are the pieces of clear reinforced hoses included with the unit(s) suitable for argon and/or compressed air?
What is the pressure rating?
Thanks!
on my 256 I use that hose only for argon and I use about a four inch run of it to feed into the machine. For the plasma, I use standard air line only UPSTREAM of the particulate filter and drier. Past that it feeds into my switching valve and then the four inch clear tube. I wouldnt run anything into the machine with a standard air hose because I cannot see through it. That's just me though. I'm not saying that the braided line cant handle shop air But the rubber hose I use is a little beefier and more flexible and I have good driers hooked up so I'm not concerned and about particulates lfowing though it that I cannot see.