Just Bought PowerTig 185
Hi all,
I'm new to welding but have been building bikes for some time (welding was done by Chassis Enginnering who are local to me). I bought a PowerTig 185 to learn how to weld on. My unit arrived in good condition, no damage from shipping. I have been using the machine a few days and it has been great. This machine is very capable and in an experienced welders hands I am sure it can make some nice beads.
Here are some pictures in my cluttered garage...
http://i13.photobucket.com/albums/a2...2-08135944.jpg
http://i13.photobucket.com/albums/a2...2-08135953.jpg
http://i13.photobucket.com/albums/a2...2-08140041.jpg
http://i13.photobucket.com/albums/a2...2-08140224.jpg
http://i13.photobucket.com/albums/a2...2-08144102.jpg
And these are some of the welds I have made with it.
http://i13.photobucket.com/albums/a2...2-09191929.jpg
http://i13.photobucket.com/albums/a2...2-11172649.jpg
-
-
That looks great for 3 days! Tie in is good, heat lines show even torch angle. Color of weld appears to be the correct temperature. Bead with is fine, with a little underfill on the sides of the bevel toward the end on the second picture. The ends of the welds look properly filled as well.
I have told many guys that this machine will meet almost all their needs. There is no slack in performance or weld quality on this unit. I can tell you that it is every bit as competent as any of our other TIG welding units.
-
How much does this machine cost with a foot pedal? I am torn between this one and the PowerTig DX 200A. I mean the 200A is only $1100. If this one is $900 shipped with a foot pedal, it is almost worth it just to get all the extra options for another $200.
-
Diabolic,
Give me a call and we'll see what we can do on a 185.
-