Originally Posted by
Wrenchtamer
just wanted to let you guys know I went to harbor freight last night and they have an air cooled tig torch (17v) with gas valve that is being discontinued and is on nationwide clearance for 1.47$. thats right. one dollar and forty seven cents. I bought the last three at my local store. It is a good torch. no strange one off part on it. I checked the power cable and it is interchangeable with the other weldcraft wp17f torch I have. it does not have a switch or a gas fitting but I thought the gas valve was cool in case I want to hook it up to my smaw power source on the truck. they also have a genuine binzel torch with a switch on it and a gas fitting but they wouldnt sell it to me. they said it only comes with the tig welder they sell. that was a badass looking little torch too. nice flexible cables and skinny little handle. I think i might try my luck again this afternoon. so check your local stores and if you dont see them ask the associate. they only had one on the shelf but thye had two more in the back. the sku is 92363 66921.