Does anyone have some good settings for your Everlast machine from 1/8th" up to 1/2" regular mild steel. I know a lot of variables go into it, just looking for some good starting points. I use to use an app on my phone my Lincoln and the setting seemed to be pretty close. However, after replacing my phone I can no longer find the app. I've tried the Miller app and the wire feed speed seems to be way off, unless it is my inexperience and i'm not moving fast enough. But I seem to get a better looking weld when I slow it down. I'm running a 251si in standard mig mode.
For example the miller app states for 1/8th" using .35 wire I would be at 280-300 ipm and 18-19 volts
When I weld at those settings I can feel the wire tapping the metal that I am working on.