After playing with the (flawless)steel mig & stick functions..the 200n arrived...set up..acetone THEN new ss wire brush in one direction...21.5 v..355 ipm..25cfh argon....Nothing but turds.....up & down the v wfs thing....same...checked argon fittings with soapy water...all good..took the feed tube out looking for crude in the port...nothing...diffuser clean...check flo but really weak....finally..back to 21.5 v..355 ipm..(my settings at work)..cranked argon up to 60 cfh.....WAY better....crank it wide open...NOW its spraying....great cleaning lines...no soot.......Which leads me to believe..Theres a restriction OR leak starting from the barb on the machine up to the gun......Any 200 dual/200N owners exp this....????...Mark...Ram..Zoama..