Looking for info on which spool gun works with the power mig 275s. The SM200N or SM200 MTS? I have two SM200N guns.
Printable View
Looking for info on which spool gun works with the power mig 275s. The SM200N or SM200 MTS? I have two SM200N guns.
SM200MTS is supposed to work with it. The 200N standard does not have amp control in the gun handle. You have to control it on the panel. The MTS does have amp control in the handle.
Performance,
Thanks for the info. But will the sm200n work with it? I had a I mig 250 which had to be controlled at the panel so that's OK, just need to know if they will work with the 275s. Thanks.
No. It won't. Not designed to.
Ugh. Now I have to see how to get another issue taken care of. Thanks