Just wanted to stop by, and tell you guys how impressed I' am with my new PowerArc 300!:cool: I've never ran much 6010 in my life, but this machine makes it about as easy as falling off a log. I know this isn't perfect, but like I said I never ran much 6010.
6-inch sch 80 pipe 6-G. Cap passes is 5/32-inch ESAB 10P 6010. Ran it at 125-amps, 5 on the arc force.