Needed a tough enclosure for a new doorbell button and gate keypad. More than one delivery driver could't find the old one and would just drive away. So I wanted something that would stand out a little. I had some leftover 14ga. treadplate that was a good starting point.
Cut out the pieces and did a little machine work, then TIG to assemble. Smooth, prime, paint, and install.
Done deal.