5 Attachment(s)
Apocalypse Stove - runs on any liquid fuel made with i MIG 200
Attachment 11043Attachment 11044Attachment 11045Attachment 11046Attachment 11047
This will boil a 1qt pan of water with a 1/4" poly rope (I just used poly to test). I have 3/8" cotton rope on the way.
I'll post more pictures once I get it going good with the 3/8" rope.
I run it on Methanol, but just about any liquid fuel can be used (I wouldn't recommend Gasoline).
8 Attachment(s)
More pictures as promised...
Hey guys,
I finally got that 3/8" cotton rope that I was waiting on.
I have the "wick" sticking out about 1-1/4"
I also added 4 more 3/8" air inlet holes to allow enough air to burn clean. :D
Attachment 11161Attachment 11162Attachment 11163Attachment 11164Attachment 11165Attachment 11166Attachment 11167Attachment 11168
My Youtube video is currently uploading (41%) as of 4:25 CDT
http://www.youtube.com/watch?v=V2ZFz...ature=youtu.be