7 Attachment(s)
Less than one year old John Deere mower repair.
Did a repair on a John Deere the guy swears he did not hit anything. Hope pictures came out OK.
Start removing parts.
Attachment 10994
Grind out hole. There was no rust.
Attachment 10993http://www.everlastgenerators.com/fo...1&d=1382281292
Tack and square up.
Attachment 10992
Weld. You can see the tear
in the metal. He must have hit
something. Cash is cash no matter.
Attachment 10995
I went over tear and did the back.
Attachment 10997Attachment 10998