Aluminum Welding with Micro185
Purchased this machine last year. i was self taught and learn alot from youtube.
picked up this machine over the 200dx last year because i didnt think i would use the machine alot
but now i been doing alot of side jobs and making catch cans for cars and planning to build turbo manifolds
planning to pick up the newer model 200dx. well here are the pics.
when i first started last year
https://fbcdn-sphotos-f-a.akamaihd.n...52867470_n.jpg
first catch can i made using 4043 filler rod
http://i14.photobucket.com/albums/a3...psddeb08e5.jpg
small catch can using 4043 filler rod
http://i14.photobucket.com/albums/a3...psce7f6ed3.jpg
http://i14.photobucket.com/albums/a3...ps12ceaa1e.jpg
http://i14.photobucket.com/albums/a3...psf9807637.jpg
2nd small catch can using 5356 filler rod(really love this stuff)
http://i14.photobucket.com/albums/a3...psd2c970d1.jpg
big catch can also using 5356
http://i14.photobucket.com/albums/a3...ps06e25cd0.jpg
close up
https://fbcdn-sphotos-h-a.akamaihd.n...19417978_n.jpg
planning to build end tanks for this 1000hp garret intercooler for my sc300
http://i14.photobucket.com/albums/a3...psb8457510.jpg
definitely a great machine, i would recommend this to anyone that want to start off welding.