I have to get a system to purge the back of SS weldments.
Option 1: Buy a dual flow meter (150-300$)
Option 2: Buy a second argon tank 150cf (300$)
Option 3: Put a brass T fitting running off the tank flow meter.
Option 4: Make an argon chamber and use a scuba tank for respiration! JK :/
Any input?