4 Attachment(s)
Two simple artwork display stands
Nothing special here. A fellow brought two bases and two tops, One I had to cut a pipe off of. It is for him to display his metal art. A couple pictures. All MIG with Everlast IMIG-250P with ER70-6, 21 volts and about 200 on the wire-feed speed. Was outside and it was windy, as you can see the spatter.
Round one
Attachment 9831
Square one, non cleaned up or painted .
Attachment 9833
Penetration, mine is outer one. It had a pipe welder to it same and the squared one.
Attachment 9832
Final product.
Attachment 9830
Will show the art later, he has us doing the artwork. If he OKs it I will post that too. All polished SS.