I have a powertig 200dx. Finally got my garage wired up and started messing around welding stuff up. I am have a couple issues though. When welding steel I get this orange coloration around the edges. It's more a soot than anything. See pic below. Next when welding aluminum I can get the arc to focus. It jumps around and leaves this black spotting. Any help or info is appreciated. I have tried different gas, tungeston, made sure everything is clean with acetone.