Winter Time Fun Contest Project #4 cbmkr Welding Repair 20 ga Car Floor Brace
Restoring my old ride and ordered some new floor braces they came without the tabs to spot weld them on. Used the 200DX set at 35 amps on DC w/6 cf gas flow and added the tabs to each floor brace. Photo shows an original that i cut from a donor car and the new ones after the tabs were added.
Attachment 9564Attachment 9565Attachment 9566Attachment 9567
I could use an MTS 160 with .023 wire to set up in the car when welding patch panels in, My millermatic 200 is a little large for that.