Suggestions on best fit for the needs of a small operation.
So I'm planning on doing a variety of work, most notably a lot of auto-related welding and cutting in the near future. The big catch is that my garage is only wired for 110, and since I'm renting I'd rather spend the money on tools than upgrading wiring for my landlord. I've got zero welding experience, but I'm hoping to pick it up quick. Future plans include welding various aluminum items I've got, so I'm thinking that means I'll need a TIG unit. I'd like to keep things small if possible, and really like the idea of a single do-all machine, but getting the best bang for my buck and hopefully having something that can weld on beefier stuff once I move out and get a place wired for 220 is important.
So with this in mind, as far as general utility 110/220, what would you guys suggest? At a glance, it doesn't look like there are any TIG/stick/plasma cutter combos that match my needs. TIG's a must, but stick capability seems like a very good idea for bulk work. I'm guessing the plasma cutter will have to be a separate unit. Are there any considerations I need to make (but haven't)?