Has a person that wanted some tools made, figure I would post the final tools. Rebar, steel plate, nuts and bolts.
One a to pickup the crucible, other to are to move and pour the metals. He invited us to come see them in action, will get more pictures then.
Attachment 8664Attachment 8663Attachment 8662
Attachment 8670Attachment 8661Attachment 8668Attachment 8665Attachment 8669
Attachment 8666Attachment 8667