Yesterday was preparing a motorcycle to practice on it Stuntriding.
Guys asked me to make strengthening of a seat rail ,also make a footboard with an insert of the titan, thus, they can make such tricks(crazy people:))Attachment 7887Attachment 7888Attachment 7889
here that turned out.(welding with рр256 gave pleasure;))
Attachment 7890Attachment 7891Attachment 7892Attachment 7893Attachment 7894
http://i1203.photobucket.com/albums/...r1976/0632.jpg
http://i1203.photobucket.com/albums/...r1976/0640.jpg
http://i1203.photobucket.com/albums/...r1976/0641.jpg
http://i1203.photobucket.com/albums/...r1976/0642.jpg
http://i1203.photobucket.com/albums/...r1976/0643.jpg
http://i1203.photobucket.com/albums/...r1976/0647.jpg
http://i1203.photobucket.com/albums/...r1976/0650.jpg
http://i1203.photobucket.com/albums/...r1976/0653.jpg