Hello all,
I have a PP50. It has worked flawlessly until today. The last use was a week or so ago. It worked fine. I finished the cuts, let the fan run for a few and then shut the machine down. Today I went out to make some cuts and.....Problem!
Turned machine on, All is well.
Checked air pressure, all is well.
Grounded the metal, pulled the trigger, I got air flow, but no pilot arc or cutting.
Checked the swirl ring, all is well.
Replaced the electrode, same thing.
replaced the tip, same thing.
Adjusted post flow, switched from constant to timed and back several times, no change.
Switched from 2T to 4T and back, no change.
Is there an adjustment for the pilot arc? like a contact gap or something?
My machine sits on a dedicated cart with a dedicated air line, hard wired by an electrician.
Any help is appreciated.