I've been using my IMIG200 with .030 wire in it, 2lb. spools. I'm almost out of my last 2lb. .030 wire and I have an 11lb. roll of .035.
The .030 wire is all I've used in this welder so this is why I'm asking about the .035.
I weld thinner material, 1/16", 1/8"..maybe 3/16"... Will the .035 wire be ok to run or should I save it and go get some .030?
I just don't want to load an 11lb. spool and then have to take it out mid roll if it doesn't work for me...