Power I-MIG 205 should name it the super flame thrower lol
Well finally had a break at the shop to set up the Power I-MIG 205 . hooked up the gas and threw a 33 pound roll of .035 in it . tossed some 1/4 plate and had a piece of 1/2 . did some beads took a few minutes to get dialed in on the controls since different than my other mig . Wow talk about penetration and throwing some heat out can tell this welder would love .045 lol .. Thanks Alex nice finally having a mig with some heat and power for thick stuff the 175hd Lincoln just didn't have the power for 3/16 or thicker metal . Also was nice when you get the weld it comes with the connection for the spool gun so you have a plug for it . . Did pull the cover before using only because there was chunks of Styrofoam in the air valve port and had to remove to get the foam chunks out of it , looked very well made inside . nice now i have my small welder for exhaust and thin stuff and don't have to switch rolls of wire all the time with 2 machines now.