I'm currently welding up a heat exchanger for a local microdistillery. Everything is welded at around 100-120 amps on my powerultra 205p. Cu to stainless with silicon bronze rods, stainless to stainless with 308 rods, 100% Ar. Pulsing on the copper to ss welds.