2 Attachment(s)
My first official use of my 250EX
Attachment 6286Well I got a 250EX recently and did some quick beads on Al, but this weekend came time to convince the wife that this purchase will "pay off" in time as a household repair of our "love seat" was in order. Two spring supports broke. I used my FR cover alls to prevent the place from possible burning down with an extinguisher and pails of water close by.
Attachment 6285
I left the cooler in the garage due to the lower current for this repair.I took the opportunity to strengthen the wooden sections with more bracing.