3 Attachment(s)
First prototype portable flywheel grinding machine
Love free time to work on projects. have some funny car racers that gave me some hints on a machine to resurface there clutch plates and floater on the clutch pack units so got down and built a grinder they would like and also was a wet grinder since not so messy and leaves a perfect finish on there floaters with out plates warping . well got 1st design done . post some pics Attachment 6056Attachment 6057Attachment 6058Attachment 6059