all the rating i see are 15-20 cfh..
my harris regulator came with my lincoln 180c, it has
L/MIN and SCFH and im using it on my argon tank too.
so what should i be at in either L/MIN or SCFH?
Printable View
all the rating i see are 15-20 cfh..
my harris regulator came with my lincoln 180c, it has
L/MIN and SCFH and im using it on my argon tank too.
so what should i be at in either L/MIN or SCFH?
i usually tig weld between 4-7 LPM.
The first time I set the flow on the gauge-type regulator that came with my mig, I didn't realize the outer scale was in L/Min and not CFH. I was running 20 L/min for the first few days until I actually looked closely at it.