Are there major differences in rod quality between brands? For the anticipated arrival of my PA200, I bought Hobart 6011, 6013, and 7014. I declined to buy the rod that Harbor Freight was selling just out of principle, although I did walk out with an auto-darkening helmet.
thanks,
Ian