Here at my school things are always being improved (welders equipment etc) We received 3 tanks that are going being used as quench bins. I was assigned to fabricate running gear to the bottoms of the carts. Here are some pictures of the project
Here are some of the unsuspecting components
http://oi56.tinypic.com/n2n7fc.jpg