  1. Tig welding .032 aluminum

    I have a dv200 tig on 110v. Trying to weld thin aluminum
    Butt weld and corner welds. Tried setting frequency to 210 with low cleaning at 20 percent have my Amps at 20 Amos the lowest. Argon at 15 cup#5 using gray tungsten 1/16
    Using a diffuser in the cup. Burns through the aluminum almost immediately. Looking for the best settings as I?m fairly new to tig welding. Any help would be greatly appreciated.