11-01-2024, 08:04 PM
I'm getting tired of changing these fittings. I have many welders and NEVER have broke another but on my 3rd from Everlast. I'd like to just put a...
2 replies | 120 view(s)
-
11-06-2024, 04:39 PM
The first time the fitting did not move so i assumed threaded into the body of the welder so one wrench. It snapped inside the machine. These last...
2 replies | 120 view(s)
-
11-05-2024, 08:11 PM
You can call tech support at 877 755 9353 ext 207 and they can help you.
1 replies | 73 view(s)
-
11-05-2024, 08:10 PM
9 to 10 is typical.
1 replies | 116 view(s)
-
11-05-2024, 08:05 PM
They break from over tightening. Very rare problem unless you put excessive force on it. Are you holding one side when you tighten the other as...