Things to Do for a Perfect TIG Welding


April 12th, 2010

The three things that you have to look out for that perfect TIG Welding is the length of the arc, torch angle and not shielding the hot tip of the wire.

What happens when an arc length is too long is it won’t pinpoint the heat. If you have long arc, then your TIG welding will turn to be gas welding. If you find that the tip of the rod is blobbing into the puddle, then you can identify that you arc is too long.

Same ways, too much of torch angle will even make the rod to blob. Positioning the thing that you are welding or yourself so that the torch angle is reduces and still making sure that you are able to see the tip of the electrode, is the right way to do it.

If you fail to shield the hot tip of the wire then things won’t come out well as you planned for. When you shield the tip then you can see that the puddle flows out as smooth as honey and your TIG welding will be as neat and tidy as you wanted it to be.

Share
1 Star2 Stars3 Stars4 Stars5 Stars (No Ratings Yet)
Loading ... Loading ...

Tags: , , ,

One Response to “Things to Do for a Perfect TIG Welding”

  1. Marna Gabbett says:

    I have been previously watching the website for the month or so and also have found a heap of effective details. I’m undertaking to run my own blog nevertheless It looks like its too basic and I would like to concentrate more about smaller subjects.

Leave a Reply