  • Simultaneously we can make any number welds in heavier materials easily.
  • Projection welds can be made in metals that are too thick to be joined by spot welding.
  • When you compare with spot welding, projection welding interferes less scale, oil, rust and work metal coatings.
  • Lower Electrode Maintenance.
  • Less Welding Current Required.
  • Projection welding life is longer than spot welding.
  • Lower amount of current and pressure needs to joint metals.