  • While welding or cutting in confined space, the space should be cleaned, ventilated and tested during the welding operation.
  • The way of entering a confined space, should be quickly removing employee in case of an emergency.
  • When arc welding in a confined space is to be suspended for any substantial period of time all electrodes should be removed from the welders and the machine shut off.
  • When gas welding or cutting in a confined space is to be stopped for any substantial period of time the torch valves should be closed and the machine shut off. The welding torch and hose shall be removed from the confined space or disconnected from the gas supply during welding. Before re-entering in confined space atmospheric tests shall be made.
  • Check whether hoses and connections are free from leaks.
  • When gas welding or cutting in a confined space, such as pipe line, compartment, tank or container, check to be free from explosive vapors or any danger of explosion.
Share
1 Star2 Stars3 Stars4 Stars5 Stars (No Ratings Yet)
Loading ... Loading ...

Tags: ,

7 Responses to “Precautions in Confined Spaces While Welding Or Cutting”

  1. WP Themes says:

    Amiable brief and this fill someone in on helped me alot in my college assignement. Gratefulness you as your information.

  2. WP Themes says:

    Amiable post and this mail helped me alot in my college assignement. Thanks you as your information.

  3. table decoration says:

    I really liked reading your post!. Quallity content. With such a valuable blog i believe you deserve to be ranking even higher in the search engines :) . Check out the link in my name. That links to a tool that really helped me rank high in google. This way even more people can enjoy your posts and nothing beats a big audiance ;)

  4. quick loan says:

    hey there I just wanted to comment your blog and say that I really enjoyed reading your blog post here. It was very informative and I also digg the way you write! Keep it up and I’ll be back to read more soon mate

  5. wholesale sunglasses says:

    great information you write it very clean. I am very lucky to get this tips from you.

  6. Wholesale shoes says:

    good information you

    write it very clean. I am very lucky to get this tips from you.

  7. games says:

    I just happen to stumbled onto this site and it is a good article, a little on the long end of the read but pretty good one.

Leave a Reply